Light high-strength concrete and preparation method thereof

2012 
The invention discloses light high-strength concrete, which is prepared from the following raw materials in percentage by weight: 10 to 15 percent of silicate cement, 8 to 12 percent of mineral powder, 6 to 10 percent of coal ash, 2 to 6 percent of wollastonite, 20 to 30 percent of ceramsite,25 to 35 percent of ceramic sand, 0.2 to 0.8 percent of high-performance water reducing agent, 0.05 to 0.3 percent of exciting agent, 0.05 to 0.8 percent of tackifier and 8 to 12 percent of water. The light high-strength concrete has the advantages that compact accumulation is realized by optimizing the grain composition of cementing materials; the mineral powder is subjected to ultrafine grinding, so that the hydrated activity of the mineral powder is improved substantially; and the using quantity of the low-density cementing materials can be increased, and the cohesiveness of slurry is improved by combining the high-performance water reducing agent, the exciting agent and the tackifier, so that the concrete slurry is high in working performance and is not segregable, and the aim of reducing the volume weight of the hardened slurry substantially is fulfilled on the basis of ensuring the mechanical property of the hardened slurry.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    0
    References
    0
    Citations
    NaN
    KQI
    []